Processing of spent NiW/Al2O3 catalysts
AUTOR(ES)
Paulino, Jéssica Frontino, Afonso, Julio Carlos, Cunha, José Waldemar Silva Dias da
FONTE
Quím. Nova
DATA DE PUBLICAÇÃO
2013
RESUMO
Spent oxidized (500 ºC, 5 h) commercial NiW/Al2O3 catalysts were processed using two different routes: a) fusion with NaOH (650 ºC, 1 h), the roasted mass was leached in water; b) leaching with HCl or H2SO4 (70 ºC, 1-3 h). HCl was the best leachant. In both routes, soluble tungsten was extracted at pH 1 with Alamine 336 (10 vol.% in kerosene) and stripped with 2 mol L-1 NH4OH (25 ºC, one stage, aqueous/organic ratio = 1 v/v). Tungsten was isolated as ammonium paratungstate at very high yield (> 97.5%). The elements were better separated using the acidic route.
Documentos Relacionados
- Hydrogenation of 2-ethyl-hexen-2-al on Ni/Al2O3 catalysts
- Selective Hydrogenolysis of Glycerol to 1,2-Propanediol Over Bimetallic Cu-Ni Catalysts Supported on γ-Al2O3
- Cu and Ni Catalysts Supported on γ-Al2O3 and SiO2 Assessed in Glycerol Steam Reforming Reaction
- The effect of precursors salts on surface state of Pd/Al2O3 and Pd/CeO2/Al2O3 catalysts
- SÍNTESE POR REDUÇÃO IN-SITU E CARACTERIZAÇÃO MICROESTRUTURAL DOS NANO-COMPÓSITOS CU-AL2O3 E NI-AL2O3