The Production of UV Absorber Amorphous Cerium Sulfide Thin Film
AUTOR(ES)
Kariper, İshak Afşin
FONTE
Mat. Res.
DATA DE PUBLICAÇÃO
27/07/2017
RESUMO
This study investigates the production of cerium sulfide (CeSx) amorphous thin films on substrates (commercial glass) by chemical bath deposition at different pH levels. The transmittance, absorption, optical band gap and refractive index of the films are measured by UV/VIS Spectrum. According to XRD analysis, the films show amorphous structure in the baths with pH: 1 to 5. It has been observed that the optical and structural properties of the films depend on pH value of the bath. The optical band gap (2.08 eV to 3.16 eV) of the films changes with the film thickness (23 nm to 1144 nm). We show that the refractive index has a positive relationship with the film thickness, where the values of 1.93, 1.45, 1.42, 2.60 and 1.39 are obtained for the former, and 34, 560, 509, 23 and 1144 nm (at 550 nm wavelength) for the latter. We compare the optical properties of amorphous and crystal form of CeSx thin films. We show that the optical band gaps of the amorphous CeSx are lower than that of crystal CeSx.
Documentos Relacionados
- Li diffusion and electrochromism in amorphous and crystalline vanadium oxide thin film electrodes
- Thin film-XRF determination of uranium following thin-film solid phase extraction
- Thin-film ZnO/CdS/CuIn1-xGa xSe2 solar cells: anomalous physical properties of the CuIn1-xGa xSe2 absorber
- Amorphous ferrous sulfide as a reducing agent for culture of anaerobes.
- Infrared analysis of thin films: amorphous, hydrogenated carbon on silicon