1. The Modification of (Nd0.5Ta0.5)4+ Complex-Ions on Structure and Electrical Properties of Bi0.5Na0.5TiO3-BaTiO3 Ceramics
The (Bi0.5Na0.5)0.94Ba0.06Ti1-x (Nd0.5Ta0.5) xO3 (0.01≤x≤0.05) lead-free ceramics (BNBT-xNT) used (Nd0.5Ta0.5)4+ complex-ions to modify its structure and electrical properties. The BNBT-xNT ceramics exhibit the coexistence of tetragonal and rhombohedral phase. The (Nd0.5Ta0.5)4+ complex-ions prohibit grain growth, and its average grain size decreases fro
Mat. Res.. Publicado em: 14/03/2019
-
2. A Comparative Analysis of BaTiO3/(Ba,Sr)TiO3 and BaTiO3/(Ba,Sr)TiO3/SrTiO3 Artificial Superlattices via Raman Spectroscopy
BaTiO3/Ba50Sr50TiO3 and BaTiO3/Ba50Sr50TiO3/SrTiO3 superlattices are characterized via Raman spectroscopy. Special attention is paid to a comprehensive analysis of their polarized Raman spectra, especially, within a soft mode (E(1TO)) range. The shift of E(1TO) soft mode is found to be more pronounced for BaTiO3/Ba50Sr50TiO3/SrTiO3 sample than for BaTiO3/Ba5
Mat. Res.. Publicado em: 14/11/2018
-
3. Piezoelectricity from Elastic and Dielectric Measurements on Unpoled Ferroelectrics
A method is described to assess the piezoelectric response of ferroelectric materials from the temperature dependence of the elastic moduli and dielectric constant of unpoled samples. The limits and advantages over the traditional methods on poled samples are discussed. A quantitative check is made by comparing the piezoelectric softening measured below the
Mat. Res.. Publicado em: 07/06/2018
-
4. Caracterização térmica e estrutural de pós e filmes finos de BaTiO3 sintetizados via método Pechini / Thermal and structural characterization of powders and thin films of BaTiO3 synthesized by Pechini method
Amorphous oxides are chemical compositions whose atomic or molecular configuration does not follow a periodicity like it happens with crystals, which are essentially constituted by oxygen atoms, which has to be the most electronegative element, and other elements. The barium titanate (BaTiO3), amorphous oxide obtained through this work has tetragonal structu
IBICT - Instituto Brasileiro de Informação em Ciência e Tecnologia. Publicado em: 29/02/2012
-
5. Síntese, caracterização elétrica e estrutural de cerâmicas ferroelétricas de composição Ba0,90R0,10Ti1-xZrxO3 (R=Ca, Sr) / Synthesis, electric and structural characterization of Ba0,90R0,10Ti1-xZrxO3 (R= Ca, Sr) ferroelectric ceramic system
O presente trabalho teve como objetivo o estudo das propriedades elétricas e estruturais das amostras cerâmicas pertencentes ao sistema Ba1-xRxTi1-yZryO3 (R=Ca,Sr). As amostras na forma de pó micro ou nanoestruturadas foram respectivamente obtidas através do método de mistura de óxidos e do método dos precursores poliméricos. Amostras cerâmicas apre
Publicado em: 2010
-
6. Cation size effects-modified phase and PTCR development in Er3+ and Ca2+ co-doped BaTiO3 ceramics during sintering
Development of the positive temperature coefficient of resistivity (PTCR) in Er3+ and Ca2+ co-doped ferroelectric BaTiO3 was studied in this work, with Er3+ being used to act as a donor doping. Irrespective of all the materials showing high densities after sintering at 1200 to 1300 ºC, these revealed insulator at the lowest sintering temperature, changing t
Materials Research. Publicado em: 2009-09
-
7. The density effect on grain boundaries in dielectric properties and dielectric anomalies of ferroelectric ceramics of BaTiO3. / Efeito da densidade dos contornos de grãos nas propriedades e anomalias dielétricas de cerâmicas ferroelétricas de BaTiO3
Neste trabalho, cerâmicas de BaTiO3 foram preparadas pelo método de Pechini com o propósito de estudar as suas propriedades dielétricas, incluindo as anomalias dielétricas de origem interfacial nestes ferroelétricos. Após calcinação das soluções precursoras a 600 oC por 2h, os pós compactados foram sinterizados a várias temperaturas entre 1150 e
Publicado em: 2009
-
8. Synthesis and dielectric properties of the lase sintered Ba1-xCaxTiO3 (0 ≤ x ≤ 0.30) nanostructured ceramics / Síntese e propriedades dielétricas de cerâmicas nanoestruturadas de Ba1xCaxTiO3 (0 menor igual x menor igual 0.30) sinterizadas a laser
Ba1-xCaxTiO3 (0 ≤ x ≤ 0.30) nanocrystalline powders were successfully synthesized for the first time at relative low temperature (500 °C) by a modified polymeric precursor method. The densification of the ceramics was made by two distinct techniques: conventional sintering using an electric furnace; and by a laser sintering process in which a CO