1. Correlação de estrias de fadiga com espectro de cargas em liga de Al aeronáutica SAE-AMS 7475 T 7351. / Correlation of fatigue striation spacing to loading history in aeronautic Al alloy, AMS 7475 T7351.
This work discusses the relationship between striation spacing, i.e. the microscopic crack propagation rate, SL (local) e SP (projected), as measured in post-mortem fractographic inspection of fatigue fractured surfaces, and the macroscopic crack propagation rate, da/dN, as monitored during fatigue crack growth tests. Compact tensile specimens C(T) were extr
Publicado em: 2003